This is a picture of a bathroom vanity top with a crack at the back left corner. This was due to water reaching the mdf base which the corian was glued to, this is standard practise. The vanity top had a slight gap at the back and the sealer had failed. The mdf base soaked in water causing it to swell and causing the corian to crack, as the corian glued joint at the corner failed causing it to seperate. The job was in harrogate, we arrived on site and completed the repair the same day. See the finished result at worktoprepairs.com in our repair gallery.

Finished cracked corian worktop.

Back

Leave a Reply

Your email address will not be published. Required fields are marked *

This field is mandatory

This field is mandatory

This field is mandatory

There was an error submitting your message. Please try again.

Security Check

Invalid Captcha code. Try again.

©Copyright. All rights reserved.

Information icon

We need your consent to load the translations

We use a third-party service to translate the website content that may collect data about your activity. Please review the details in the privacy policy and accept the service to view the translations.